Preparation and Properties of MDI/H12MDI-Based Water-Borne Poly(urethane-urea)s-Effects of MDI Content and Radiant Exposure
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q3
- 저널
- JOURNAL OF APPLIED POLYMER SCIENCE110(6) · pp.3655 · 2008
- 피인용
- Web of Science 8
- JCR IF
- JCR 2007 1.008
- ISSN
- 0021-8995
저자
- Huh, Jae Ho제1저자Busan Branch of Korea Apparel Testing and Research Institute, South Korea
- 김혜인Department of Organic Material Science and Engineering, Pusan National University, South Korea
- 라만Department of Organic Material Science and Engineering, Pusan National University, South Korea
- 김한도교신저자Department of Organic Material Science and Engineering, Pusan National University, South Korea
초록
Water-borne poly(urethane-urea)s (WBPUs) were prepared by a prepolymer mixing process using aromatic diisocyanate (MDI, 4,4'-diphenylmethane diisocyanate)/aliphatic diisocyanate (H12MDI, 4,4'-methylenebis cyclohexyl isocyanate), polypropylene glycol (PPG, M-n = 1000), dimethylol propionic acid, and ethylene diamine as a chain extender, and triethylamine as a neutralizing agent. The effect of MDI on the molecular weight, chemical structure, dynamic thermo, and tensile properties of WBPUs was investigated. The yellowness index (YI, photo-oxidation behavior) change of WBPUs under accelerated weathering exposure was also investigated. The WBPUs containing higher MDI content showed lower molecular weight, which verified the participation of some high reactive isocyanate groups of MDI into side reaction instead of chain growing reaction. As the MDI content increased, the storage modulus and tensile modulus/strength of WBPUs film increased, and their glass transitions of soft segments (T-gs) and hard segments (T-gh) were shifted to higher temperature. The intensity of tan 6 peak of all three samples increased with increasing radiant exposure. The YI of H12MDI-based WBPU sample (WBPU-0) was not occurred. The YI of WBPUs containing MDI increased with increasing MDI content and radiant exposure. However, the YI of sample WBPU-25 containing 25 mol % of MDI at 11.3 MJ/m(2) (radiant exposure) was 6.6 which is a permissible level for exterior applications. (c) 2008 Wiley Periodicals, Inc. J Appl Polym Sci 110: 36553663, 2008
키워드
water-borne poly(urethane-urea)MDIH12MDIradiant exposureyellowness indexPOLYURETHANE SYSTEMFILMS CASTDISPERSIONSDEGRADATIONBEHAVIORS