Effect of the minimum quantity lubrication in high-speed end-milling of AISI D2 cold-worked die steel (62 HRC) by coated carbide tools
- 문서 유형
- 연구출판물 · 학술대회 발표논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1
- 저널
- SURFACE & COATINGS TECHNOLOGY202(22-23) · pp.5621 · 2008
- 피인용
- Web of Science 48
- JCR IF
- JCR 2007 1.678
- ISSN
- 0257-8972
저자
- 강명창제1저자교신저자National Core Research Center for Hybrid Materials Solution Materials, Pusan National University, South Korea
- 김광호National Core Research Center for Hybrid Materials Solution Materials, Pusan National University, South Korea
- Shin, S. H.National Core Research Center for Hybrid Materials Solution Materials, Pusan National University, South Korea
- Jang, S. H.School of Mechanical engineering, Pusan National University, South Korea
- Park, J. H.School of Mechanical engineering, Pusan National University, South Korea
- 김철Research Institute of Mechanical Technology, Pusan National University, South Korea
초록
The objective of this paper is to compare the tool performance of Ti0.75Al0.25N and Ti0.69Al0.23Si0.08N coated carbides end-mills deposited by hybrid coating method, using flood coolant(wet), dry and minimum quantity lubrication (MQL) conditions in the high-speed machining of AISI D2 cold-worked die steel (62 HRC). Superhard Ti-Al-Si-N films, characterized as a nanocomposite nano-sized (Ti,Al,Si)N crystallites embedded in amorphous Si3N4 matrix, was successfully synthesized on WC-Co substrates by a hybrid coating system of arc ion plating(AIP) and sputtering method. The hardness of Ti-Al-Si-N film increased with incorporation of Si, and had the maximum value similar to 48 GPa at the Si content of 8 at.%, respectively. The values of tool wear for coated tools were evaluated under a high-speed cutting condition using vertical high-speed machining center (Makino, V-55). It is found that cutting under flood coolant condition results in the shortest tool life due to severe thermal cracks while the use of MQL leads to the best performance. MQL is beneficial to tool life both in the Ti0.75Al0.25N and Ti0.69Al0.23Si0.08N coating tools. This conclusion proves the feasibility in the highspeed machining of high-hardened materials for industrial applications. (C) 2008 Elsevier B.V. All rights reserved.
식별자
- WoS UID
- 000260268900095



로그인