Controlling the temperature coefficient of resistance and resistivity in RuO2-TiO2 thin films by the intermixing ratios between RuO2 and TiO2
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1
- 저널
- APPLIED PHYSICS LETTERS92(18) · 2008
- 피인용
- Web of Science 12
- JCR IF
- JCR 2007 3.596
- ISSN
- 0003-6951
저자
- 권세훈제1저자교신저자Department of Materials Science and Engineering, Korea Advanced Institute of Science and Technology, South Korea
- Kang, Sang-WonDepartment of Materials Science and Engineering, Korea Advanced Institute of Science and Technology, South Korea
- 김광호School of Materials Science and Engineering, Pusan National University, South Korea
초록
The temperature coefficient of resistance (TCR) properties and resistivities, depending on the RuO2 intermixing ratios for RuO2-TiO2 thin films and their thermal stability in the temperature range of 200-700 degrees C, were investigated. The TCR values for the RuO2-TiO2 thin films ranged from -557.17 to -54.923 ppm/K for the RuO2 intermixing ratios ranging from 0.52 to 0.81, with resistivities remaining in the range of 2600-370 mu Omega cm. Moreover, the high structural stability and its stable oxide form of the RuO2-TiO2 thin films resulted in minimal change in both TCR values and resistivities even after O-2 annealing process at 700 degrees C. (C) 2008 American Institute of Physics.