Microstructures and mechanical properties of Inconel 718 welds by CO2 laser welding
- 문서 유형
- 연구출판물 · 학술대회 발표논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2
- 저널
- JOURNAL OF MATERIALS PROCESSING TECHNOLOGY201(1-3) · pp.515 · 2008
- 피인용
- Web of Science 125
- JCR IF
- JCR 2007 0.816
- ISSN
- 0924-0136
저자
- Hong, J. K.제1저자교신저자Department of Materials Processing, Korea Institute of Materials Science, South Korea
- Park, J. H.Department of Test and Evaluation, Korea Institute of Materials Science, South Korea
- Park, N. K.Department of Materials Processing, Korea Institute of Materials Science, South Korea
- Eom, I. S.Department of Materials Engineering, Pusan National University, South Korea
- Kim, M. B.Department of Materials Engineering, Pusan National University, South Korea
- 강정윤Department of Materials Engineering, Pusan National University, South Korea
초록
CO2 laser welding characteristics of Inconel 718, heat treatment effects on microstructures, and tensile/fatigue properties were researched. CO2 laser welding was carried out on 5 mm thick plates having two different grain sizes, ASTM #4 and #10. For the fine-grain sized specimens (ASTM #10), the optimum laser welding conditions without defects were 6 kw with 2.5 m/min and 8kW with 4.0 m/min. However, on the heat-affected zone (HAZ) of large-grained Inconel 718 (ASTM #4), the microfissures were shown at the same welding conditions. Before welding, plates were pre-heat treated at three different conditions: as-received, 955 degrees C solution treatment, and 955 degrees C solution treatment+aging (955STA). After welding, welds were subjected to four different post-weld heat treatment conditions: as-welded, 955 degrees C solution treatment+aging, modified cyclic solution treatment, and direct aging (DA) treatment. In this research, modified cyclic solution heat treatment showed reduction of microfissures and improved tensile and fatigue properties. (c) 2007 Elsevier B.V. All rights reserved.
식별자
- WoS UID
- 000255737600096



로그인
연구물 목록으로