Initial stages of ruthenium film growth in plasma-enhanced atomic layer deposition
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1
- 저널
- JOURNAL OF THE ELECTROCHEMICAL SOCIETY155(5) · pp.H296 · 2008
- 피인용
- Web of Science 42
- JCR IF
- JCR 2007 2.483
- ISSN
- 0013-4651
저자
- 권세훈제1저자교신저자Department of Materials Science and Engineering, Korea Advanced Institute of Science and Technology, South Korea
- Kwon, Oh-KyumDepartment of Materials Science and Engineering, Korea Advanced Institute of Science and Technology, South Korea
- Kim, Jin-HyockHynix Semiconductor, Incorporated, Research and Development Division, South Korea
- Oh, Heung-RyongDepartment of Materials Science and Engineering, Korea Advanced Institute of Science and Technology, South Korea
- 김광호School of Materials Science and Engineering, Pusan National University, South Korea
- Kang, Sang-WonDepartment of Materials Science and Engineering, Korea Advanced Institute of Science and Technology, South Korea
초록
The initial stages of ruthenium film growth in plasma-enhanced atomic layer deposition (PEALD) on titanium nitride (TiN) substrate were investigated in detail. During the initial stages of ruthenium film growth, the influence of the substrate surface was significant and controlling thickness by counting the number of deposition cycles is no longer valid. The time required for saturated adsorption of Ru(EtCp)(2) as well as the amount of deposited ruthenium atoms per cycle changed during the initial stage. The time required for saturated adsorption of Ru(EtCp)(2) on homogeneous ruthenium surfaces was 7 s. However, it increased up to 25 s during the initial stage of the ruthenium film growth where the film growth on heterogeneous TiN substrate is dominant. By considering these changes during the initial stages of ruthenium PEALD growth, the full coverage of PEALD ruthenium can be obtained at a minimum thickness of 2.7 nm. (C) 2008 The Electrochemical Society.
식별자
- WoS UID
- 000254779700064



로그인
연구물 목록으로