Fabrication and structural analysis of aromatic polyimide ultra-thin films with different fluorine contents
- 문서 유형
- 연구출판물 · 학술대회 발표논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q3
- 저널
- COLLOIDS AND SURFACES A-PHYSICOCHEMICAL AND ENGINEERING ASPECTS313 · pp.585 · 2008
- 피인용
- Web of Science 3
- JCR IF
- JCR 2007 1.601
- ISSN
- 0927-7757
저자
- Kang, Yun Ji제1저자Department of Polymer Science and Engineering, Pusan National University, South Korea
- 김화정Department of Polymer Science and Engineering, Pusan National University, South Korea
- Kim, EunjuDepartment of Polymer Science and Engineering, Pusan National University, South Korea
- 김일Department of Polymer Science and Engineering, Pusan National University, South Korea
- 하창식교신저자Department of Polymer Science and Engineering, Pusan National University, South Korea
초록
The structural characterizations of aromatic polyimide (PI) ultra-thin films with different fluorine contents were studied. Three types of polyamic acid (PAA) were produced from polymerization of biphenyl dianhydride (BPDA)/4,4'-oxydianiline (ODA), BPDA/2,2'-bis(trifluromethyl)benzidine (TFDB), and 4,4'-(hexafluoro isopropylidene)-diphthalic anhydride (6FDA)/TFDB in N,N-dimethylacetamide (DMAc). Polyamic acid alkyl salts (PAAS) using O,O',O ''-trihexadecanoyl-triethanolamine were transferred onto a Si-wafer substrate to prepare Langmuir-Blodgett (LB) films. The behaviors of PAAS monolayers at the air/water interface were confirmed with pi-A isotherms and Brewster Angle Microscopy (BAM) images. The behaviors of PAAS monolayers at the air/water interface depend on the fluorine contents. As there is more fluorine in the main chain of PAAS, the area per molecule of each monolayer was increased. The structure of PAAS LB films with 10, 20, 30, and 40 layers on a substrate were investigated by UV-vis spectroscopy, X-ray diffraction (XRD), X-ray reflectivity, and IR spectroscopy. The obtained PAAS LB films were imidized with a thermal treatment at 300 degrees C. The imidization of PI ultra-thin film was identified by IR spectrum. Atomic force microscopy (AFM) images showed that the particle size of PI ultra-thin films on a Si-wafer were about 7-25 nm. (C) 2007 Elsevier B.V. All rights reserved.
키워드
Langmuir-Blodgett (LB)polyamic acidpolyimidefluorineLANGMUIR-BLODGETT-FILMSACID ALKYLAMINE SALTSTERT-AMINE SALTSMONOLAYERSCHAINS