Fracture characteristics of TMCP and QT steel weldments with respect to crack length
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널
- MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING434(1-2) · pp.365 · 2006
- 피인용
- Web of Science 25
- ISSN
- 0921-5093
저자
- Shin, Y. T.제1저자교신저자Department of Welding Research, Samsung Heavy Industries Co. Ltd., South Korea
- 강성원Naval Architecture and Ocean Engineering, Pusan National University, South Korea
- Lee, H. W.Research Center, Hanjin Heavy Industries, South Korea
초록
This experimental investigation focuses on an evaluation of fracture characteristics of API 2W Gr.50 (TMCP) and 580 MPa class high-strength steel (QT) weldments with respect to crack length to width ratio. Crack tip opening displacement (CTOD) values from single edge notched bending (SENB) specimen are associated with the Charpy toughness of root weld located at the middle of the specimen thickness and showed lower toughness values according to the increasing crack length to width ratio. In fractography analysis, there is no significant effect of crack tip constraint on fracture mode. The hardness values of the reheated zone in weld metal are lower than the solidified zone, and fractures are initiated at the reheated zone with low hardness values within the center third of section thickness. (c) 2006 Elsevier B.V. All rights reserved.
식별자
- WoS UID
- 000240896400052



로그인
연구물 목록으로