Tuning mechanical, oxidation, wear and cutting properties of AlTiMoN coatings via Mo content variation in HiPIMS
- Document Type
- Publications · Journal Article
- Registered DB
- SCIEScopus
- Journal Ranking
- JCR Q1Scopus Q1
- Journal
- CERAMICS INTERNATIONAL2026
- Citation
- Scopus 0
- JCR IF
- JCR 2024 5.6
- ISSN
- 0272-8842
Authors
- Zhang, HaoqiangFirst authorCorresponding authorSchool of Materials Science and Engineering, Henan University of Science and Technology, Luoyang, 471023, China
- Guo, LeipingSchool of Materials Science and Engineering, Henan University of Science and Technology, Luoyang, 471023, China
- Geng, DongsenCorresponding authorOKE Precision Cutting Tools Co., Ltd., Zhuzhou 412000, China
- Guo, XinboSchool of Materials Science and Engineering, Henan University of Science and Technology, Luoyang, 471023, China
- Xiao, ChenguangSchool of Materials Science and Engineering, Henan University of Science and Technology, Luoyang, 471023, China
- Chen, ChongSchool of Materials Science and Engineering, Henan University of Science and Technology, Luoyang, 471023, China
- Mao, FengSchool of Materials Science and Engineering, Henan University of Science and Technology, Luoyang, 471023, China
- Xu, LiujieSchool of Materials Science and Engineering, Henan University of Science and Technology, Luoyang, 471023, China
- Wei, ShizhongCorresponding authorHenan International Joint Laboratory of High Temperature Refractory Metal Materials, Henan University of Science and Technology, Luoyang, 471000, China
- Kim, Kwang HoGlobal Frontier R&D Center for Hybrid Interface Materials, Pusan National University, Busan 609-735, Republic of Korea.
Abstract
Mo alloying enhances AlTiN coatings, yet the trade-offs among mechanical, oxidation, wear, and cutting performance with varying Mo content remain inadequately understood. We investigate AlTiMoN coatings with 0–15.1 at.% Mo deposited by HiPIMS. All coatings maintain a face-centered cubic structure. Mo addition refines grains and densifies microstructure, but higher Mo levels induce nitrogen vacancies and Mo2N precipitation. Hardness peaks at 35.5 GPa with 3.4 at.% Mo, whereas fracture toughness decreases with Mo content. Mo transforms the oxide scale from a bilayered Al2O3/TiO2 structure into a dense, Al-rich scale, reducing thickness from ∼540 nm to ∼165 nm at 850 °C. Mo forms a lubricious tribofilm that lowers the friction coefficient from 0.66 to 0.51, reducing the wear rate by two orders of magnitude to 3.49× 10−8 mm3/(N·m). At 800 °C, AlTiMoN_1# shows the lowest wear rate of 1.33 × 10−5 mm3/(N·m), while excessive Mo addition leads to higher wear rates than Mo-free AlTiN due to mechanical degradation and MoO3 volatilization. Turning tests confirm that Mo-containing tools exhibit suppressed crater wear and thermal deformation, extending tool life, with AlTiMoN_1# achieving the best performance. This work establishes a comprehensive composition–performance relationship for AlTiMoN coatings and offers design guidelines for advanced nitride coatings.
Keywords
AlTiMoN coatingsCutting performanceHiPIMSOxidationWear resistance
Identifiers
- Scopus EID
- 2-s2.0-105050727769



Login