Effect of Nitrogen Addition on Martensitic Transformation and Hydrogen Embrittlement Behavior in Cold-Drawn Austenitic Stainless Steels
냉간 인발된 오스테나이트계 스테인리스강에서 질소 첨가에 따른 마르텐사이트 변태 및 수소취성 거동 변화
- Document Type
- Publications · Journal Article
- Registered DB
- KCISCIEScopus
- Journal Ranking
- JCR Q3Scopus Q3KCI Q1
- Journal
- Korean Journal of Metals and Materials64(7) · pp.644 · 2026
- Citation
- Scopus 0KCI 0
- FWCI (Scopus)
- 0
- JCR IF
- JCR 2024 1.4
- ISSN
- 1738-8228
Authors
- Cheon, HaeunFirst authorSchool of Materials Science and Engineering, Pusan Nat. Univ., Busan, 46241, Republic of Korea
- Hong, Sung-KyuRhinox Co., Ltd., Busan 46942, Republic of Korea
- Kim, Sung-HwanCorresponding authorDongnam Regional Division, Korea Institute of Industrial Technology, Busan 46938, Republic of Korea
- Hong, Seong-PakBugok Stainless Co., Ltd., Busan 46747 Republic of Korea
- Lee, Wook JinCorresponding authorSchool of Materials Science and Engineering, Pusan Nat. Univ., Busan, 46241, Republic of Korea
Abstract
Hydrogen embrittlement (HE) resistance of cold-drawn austenitic stainless steels was investigated by comparing STS316L and high-nitrogen stainless steel under identical cold drawing and high-pressure gaseous hydrogen charging conditions (10 MPa, 150°C, 600 h). Microstructural characterization, slow strain rate tensile (SSRT) tests, thermal desorption spectroscopy (TDS), and fractographic analysis were conducted to examine the effects of compositional differences on strain-induced martensite formation, hydrogen trapping behavior, and deformation characteristics. X-ray diffraction analysis revealed that both steels showed no detectable martensite after cold drawing. After SSRT, the a'-martensite fraction was 39 vol% in STS316L and 28 vol% in high-nitrogen stainless steel, indicating that the compositional differences of high-nitrogen stainless steel, including higher austenite stability, suppressed strain-induced martensitic transformation. The relative reduction of area (RRA) was 91% for STS316L and 100% for high-nitrogen stainless steel, demonstrating superior HE resistance of the high-nitrogen steel. TDS analysis showed that high-nitrogen stainless steel exhibited a higher total diffusible hydrogen content (6.65 wtppm) compared to STS316L (4.72 wtppm), yet maintained greater HE resistance. Peak deconvolution revealed that STS316L exhibited greater concentration of desorption in the high-temperature region, suggesting differences in the binding energy distribution of hydrogen trap sites between the two steels, consistent with the higher a'-martensite fraction observed after SSRT. These findings suggest that the superior HE resistance of high-nitrogen stainless steel is associated with suppression of martensitic transformation and reduction of high-energy trap site density through its overall compositional design, supporting its potential as a structural material for hydrogen infrastructure applications.
Keywords
Cold drawingHydrogenHydrogen embrittlementNitrogenStainless steel