Cryogenic properties during quasi-static and dynamic loading of high-manganese steel (13, 18.5, and 24 wt% Mn) fabricated by directed energy deposition
- Document Type
- Publications · Journal Article
- Registered DB
- SCIEScopus
- Journal Ranking
- JCR Q2Scopus Q2
- Journal
- MATERIALS TODAY COMMUNICATIONS49 · 2025
- Citation
- Web of Science 2Scopus 3
- FWCI (Scopus)
- 0.53
- JCR IF
- JCR 2024 4.5
- ISSN
- 2352-4928
Authors
- Ha, Hyeong-JinFirst authorKorea Maritime & Ocean Univ, Dept Ocean Adv Mat Convergence Engn, Busan 49112, South Korea
- Park, Han-ByeolKorea Maritime & Ocean Univ, Dept Ocean Adv Mat Convergence Engn, Busan 49112, South Korea
- Shin, Kwang-YongKITECH, Automot Mat & Components R&D Grp, Gwangju 61007, South Korea
- Lee, Wook JinPusan Natl Univ, Sch Mech Engn, Busandaehak Ro 63beon gil, Busan 46241, South Korea
- Park, SanghuPusan Natl Univ, Sch Mech Engn, Busandaehak Ro 63beon gil, Busan 46241, South Korea
- Shim, Do-SikCorresponding authorKorea Maritime & Ocean Univ, Dept Ocean Adv Mat Convergence Engn, Busan 49112, South Korea
Abstract
High-Mn steel (HMS) has an excellent work-hardening capacity and good mechanical properties, even in cryogenic environments. This study investigates the influence of Mn content on the mechanical properties of HMS fabricated by directed energy deposition (DED), focusing on their tensile and impact performances at a cryogenic temperature. HMS samples with Mn contents of 13, 18.5, and 24 wt% were deposited using the DED. The DED process parameters were optimized to minimize the gas pores, lack-of-fusion, and oxide defects. At room temperature, the hardness was the highest at 13 wt% Mn (298 HV) and decreased with increasing Mn content. This is attributed to a reduction in the martensite phase fraction. In addition, toughness and elongation increased with increasing Mn content. Importantly, the ultimate tensile strengths of the samples containing 18.5 and 24 wt% Mn were higher at cryogenic temperatures than at room temperature; however, their elongations were lower. This is because mechanisms such as twinning and transformation-induced plasticity induce stable microstructures (e.g., austenite) and phase transformations, which significantly affect ductility and toughness. Impact toughness increased with increasing Mn content at both room and cryogenic temperatures. These findings provide valuable insights into the cryogenic mechanical performances of additively manufactured HMS and support its applicability for structural use in extreme environments.
Keywords
Charpy propertiesCryogenic temperatureDirected energy deposition (DED)High-manganese steel (HMS)Tensile properties