Study on Interface and Low Temperature Sealing Capability of Thermally Aged CR (Chloroprene Rubber) O-ring
- Document Type
- Publications · Journal Article
- Registered DB
- ESCIKCI
- Journal Ranking
- JCR Q4KCI Q4
- Journal
- 엘라스토머 및 콤포지트60(1) · pp.11 · 2025
- Citation
- KCI 0
- JCR IF
- JCR 2024 1
- ISSN
- 2092-9676
Authors
- Jin Hyok LeeFirst author한국소재융합연구원
- Myung Chan Choi한국소재융합연구원
- 윤유미한국소재융합연구원
- Yongsu Jo한국소재융합연구원
- Yongwon Cho한국소재융합연구원
- Sung Han ParkAgency for Defense Development
- Kim, WonhoPusan National University
- 배종우Corresponding author한국소재융합연구원
Abstract
In this study, we observed the effect of thermal degradation on the low-temperature sealing capability. A large- sized CR O-ring of 90.0 mm inner diameter and 7.0 mm cross-sectional diameter was used. In FT-IR spectroscopy, the aged CR O-ring, CR-10, showed a carboxyl group upon oxidation. Through oxidation, the sealing force of the aged CR O-rings decreased with an increase in the degree of degradation. As the degree of degradation increased, the 10% compressive modulus had higher values at each relative position. Oxidation was caused by oxygen diffusion to the CR interface. As the degree of degradation increased, glass transition temperature (Tg) was increased, and tan δ was decreased. CR-10 showed -44.0℃ of Tg and 0.89 of tan δ. With an increase in the degree of degradation, the mobility of the CR decreased and showed a slow recovery rate at low temperatures. All specimens showed lower temperature retraction 10 (TR10) than Tg with 2.0-2.5℃ difference. The gas leakage temperature increased with the degree of degradation. This coincided with Tg and TR10 tendency. Under Tg and TR10, CR could still exhibit viscoelastic properties and could be used as a seal. At the gas leakage temperature, the CR changed to a glassy state, and leakage occurred.
Keywords
CR O-ringLow temperature sealing capabilityTemperature retraction (TR)Glass transition temperature (Tg)Modulus profiles