Phase Formation, Residual Stress, and Surface Energy of Carbon-Doped TiZrN Coatings
- Document Type
- Publications · Journal Article
- Registered DB
- SCIEScopus
- Journal Ranking
- JCR Q3Scopus Q2
- Journal
- JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE33(24) · pp.13993 · 2024
- Citation
- Web of Science 1Scopus 2
- FWCI (Scopus)
- 0.18
- JCR IF
- JCR 2023 2.2
- ISSN
- 1059-9495
Authors
- Lee Seung JaeFirst authorPusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
- Kim Seong HoonPusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
- Hong, EunpyoKorea Testing Lab, Mech & Mat Technol Ctr, Jinju 52852, South Korea
- Choi, YoungkueKorea Testing Lab, Mech & Mat Technol Ctr, Jinju 52852, South Korea
- Cho, HyunPusan Natl Univ, Dept Nanomechatron Engn, Busan 46241, South Korea
- Jo, IlgukDong Eui Univ, Dept Adv Mat Engn, Busan 47340, South Korea
- Lee, HeesooCorresponding authorPusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
Abstract
We investigated the relationship between the surface energy, phase formation, residual stress, and wettability of carbon-doped TiZrN coatings. Carbon-doped TiZrN coatings were prepared via laser ablation by controlling the thickness of the carbon paste. The crystal structure analysis revealed that the (111) plane peak shifted to a lower angle as the paste thickness increased. Lattice expansion was confirmed through Rietveld refinement, and the lattice constant of the coating increased from 4.17 to 4.41 Å. Based on X-ray photoelectron spectroscopy, it was confirmed that the formation of carbide (TiC, ZrC) phase was 4.85% for a paste thickness of 100 μm, and 12.10% for a paste thickness of 180 μm. The TiC/ZrC ratio also increased with paste thickness. The increase in carbide formation was attributed to the initial carbon concentration, whereas the increase in the TiC/ZrC ratio was ascribed to the reduction of high-energy carbon, which was sufficient to form ZrC bonds by plasma shielding. The residual stress was calculated to increase from 4439 to 5861 MPa using the sin2 ψ method. The contact angle of water decreased from 95.9° to 74.75° and that of diiodomethane decreased from 46.75° to 36.65° after carburization. With carburization, an improvement in wettability was observed for both polar and dispersive liquids, with the surface energy increasing from 36.42 to 46.24 mN/m.
Keywords
carbides formationcarbon-doped TiZrN coatingscarburization behaviorpolar and nonpolar surface energiesresidual stressWEARTIN
Identifiers
- Scopus EID
- 2-s2.0-85179677778
- WoS UID
- 001124699800003



Login
Back to Publication list