Effect of substrate preheating on the microstructure and bending behavior of WC-Inconel 718 composite coating synthesized via laser directed energy deposition
- Document Type
- Publications · Journal Article
- Registered DB
- SCIEScopus
- Journal Ranking
- JCR Q1Scopus Q1
- Journal
- INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS115 · 2023
- Citation
- Web of Science 30Scopus 28
- FWCI (Scopus)
- 1.89
- JCR IF
- JCR 2022 3.6
- ISSN
- 0263-4368
Authors
- HE SHANSHANFirst authorPusan Natl Univ, Grad Sch Mech Engn, Busandaehak ro 63beon gil, Busan 46241, South Korea
- Park, SanghuCorresponding authorPusan Natl Univ, Grad Sch Mech Engn, Busandaehak ro 63beon gil, Busan 46241, South Korea
- Shim, Do-sikCorresponding authorKorea Maritime & Ocean Univ, Dept Ocean Adv Mat Convergence Engn, 727 Taejong ro, Busan 49112, South Korea
- Yao, ChangliangKorea Maritime & Ocean Univ, Dept Ocean Adv Mat Convergence Engn, 727 Taejong ro, Busan 49112, South Korea
- Li, MingchuanHarbin Inst Technol, State Key Lab Adv Welding & Joining, Harbin 150001, Peoples R China
- Wang, ShuanglongMax Planck Inst Polymer Res, Ackermannweg 10, D-55128 Mainz, Germany
Abstract
In this study, a substrate is reinforced with WC/Inconel 718 composite coating via directed energy deposition (DED). During the DED, the substrate was preheated to 300 °C and 500 °C. The microstructural characteristics of the matrix, fusion area, and area around the WC particles were systematically investigated. The results showed that the depth of the transition zone at the interface of the deposited layer and substrate for preheating to 500 °C increased, enhancing the metallurgical bonding between the deposited layer and the substrate. Additionally, three different types of WC particle diffusion mechanisms were exhibited: (i) slight dissolution diffusion for non-preheating sample, (ii) dissolution-diffusion fragmentation for 300 °C-preheating sample, and (iii) disintegration and diffusion for 500 °C-preheating sample. In contrast, the effects of dispersion and solid solution strengthening are more pronounced than that of the microstructure coarsening caused by preheating, resulting in a higher hardness value of 384.0 HV0.1 (preheating at 300 °C) and 381.3 HV0.1 (preheating at 500 °C) compared to that of the non-preheated sample (358.9 HV0.1). Furthermore, the bending fracture of the WC/Inconel 718 composite layer exhibited typical pseudo-ductile behavior with premature fracture. Consequently, the highest bending strength occurred at preheating 500 °C, in which the maximum bending load and the displacement at the initial crack increased by 9.15% and 39.69%, respectively, compared with the non-preheated sample. Additionally, the fracture mechanism exhibited mainly intergranular fracture and less transgranular fracture.
Keywords
Bending testDirected energy depositionSubstrate preheatingWCSTRENGTHALLOY
Identifiers
- Scopus EID
- 2-s2.0-85164225546
- WoS UID
- 001041831400001



Login
Back to Publication list