Effects of Ce content on the modification of Mg 2 Si phase in Mg-5Al-2Si alloy
- Document Type
- Publications · Journal Article
- Registered DB
- SCIEScopus
- Journal Ranking
- JCR Q1Scopus Q1
- Journal
- JOURNAL OF MAGNESIUM AND ALLOYS11(7) · pp.2299 · 2023
- Citation
- Web of Science 28Scopus 30
- FWCI (Scopus)
- 2.16
- JCR IF
- JCR 2022 17.6
- ISSN
- 2213-9567
Authors
- Hu, BoFirst authorShanghai Jiao Tong Univ, Sch Mat Sci & Engn, Natl Engn Res Ctr Light Alloy Net Forming, Shanghai 200240, Peoples R China
- Zhu, Wen-JiePusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
- Li, Zi-XinShanghai Jiao Tong Univ, Sch Mat Sci & Engn, Natl Engn Res Ctr Light Alloy Net Forming, Shanghai 200240, Peoples R China
- Lee, Seul BiPusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
- Li, De-JiangCorresponding authorShanghai Jiao Tong Univ, Sch Mat Sci & Engn, Natl Engn Res Ctr Light Alloy Net Forming, Shanghai 200240, Peoples R China
- Zeng, Xiao-QinShanghai Jiao Tong Univ, Sch Mat Sci & Engn, Natl Engn Res Ctr Light Alloy Net Forming, Shanghai 200240, Peoples R China
- Choi, Yoon SukCorresponding authorPusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
Abstract
The effect of Ce content (0–1.6 wt.%) on the modification of Mg2Si phase in the as-cast Mg-5Al-2Si alloy was investigated. The original Chinese script type Mg2Si phase was refined distinctly and transformed to dispersive block shape gradually by adding Ce element. The length of Chinese script type Mg2Si phase was reduced from 110 to 50 μm with increasing Ce content to 1.6 wt.%. The results calculated by Pandat software indicated that the added Ce element first combined with Si to form CeSi2 phase, which could serve as the heterogeneous nucleation of Mg2Si phase due to the small lattice mismatch of 7.97%. The modification of Mg2Si phase was mainly attributed to the facts that Ce changed the growth steps of Mg2Si phase and CeSi2 promoted the nucleation of Mg2Si phase. With increasing Ce content from 0 wt.% to 1.6 wt.%, the YS, UTS and EL at 150 °C were improved from 67.7 MPa, 91.2 MPa and 1.6% to 84.2 MPa, 128 MPa and 7.5%, respectively.
Keywords
Heterogeneous nucleationMechanical propertiesMg-Al-Si alloysMg2Si modificationMECHANICAL-PROPERTIESMG2SI MORPHOLOGYMAGNESIUM ALLOYSMICROSTRUCTURESRSBSILICONCA