Synthesis and characterization of thermally cross-linkable poly (iminoarylene)-based hole injection layer for solution-processed organic light-emitting diodes

Document Type
Publications · Journal Article
Registered DB
SCIEScopus
Journal Ranking
JCR Q1Scopus Q1
Citation
Web of Science 9Scopus 9
FWCI (Scopus)
0.45
JCR IF
JCR 2022 15.1
ISSN
1385-8947

Authors

  1. Kwak, Seon LeeFirst authorPusan Natl Univ, Chem Inst Funct Mat, Busan 46241, South Korea
  2. Park, Hea JungPusan Natl Univ, Chem Inst Funct Mat, Busan 46241, South Korea
  3. Jang, Jae-HoPusan Natl Univ, Chem Inst Funct Mat, Busan 46241, South Korea
  4. Jeong Yong ParkPusan Natl Univ, Chem Inst Funct Mat, Busan 46241, South Korea
  5. Park, Jong MokKorea Res Inst Chem Technol, Res Ctr Adv Specialty Chem, Ulsan 44412, South Korea
  6. Lee, JihoonKorea Natl Univ Transportat, Dept Polymer Sci & Engn, Chungju 27469, South Korea
  7. Hwang, Do-HoonCorresponding authorPusan Natl Univ, Chem Inst Funct Mat, Busan 46241, South Korea

Abstract

© 2022 Elsevier B.V.A cross-linkable poly(iminoarylene), poly[(9,9-dioctyl-N-(p-tolyl)-9H-fluoren-2-amine)–co-(9,9-bis(4-(bicyclo[4.2.0]octa-1(6),2,4-trien-7-yloxy)phenyl)-N-(p-tolyl)-9H-fluoren-2-amine)] [poly(FA-co-BFA)], was synthesized as a hole injection layer (HIL) for solution-processed organic light-emitting diodes (OLEDs). Poly(FA90-co-BFA10) containing 10 mol% of benzocyclobutene (BCB) which is a thermally curable functional group was used in this study. The highest occupied molecular orbital (HOMO) and lowest unoccupied molecular orbital (LUMO) energy levels of poly(FA90-co-BFA10) were measured to be −5.14 and −2.31 eV, respectively. After heating at 150 °C for 40 min, the spin-cast poly(FA90-co-BFA10) film became completely crosslinked without requiring the use of additional initiators. The crosslinked thin film showed good film-forming properties and excellent solvent resistance (up to 99 %). A photo-crosslinked poly[bis(4-butypheny)-bis(phenyl)benzidine] (poly-TPD) was used as the hole-transporting layer (HTL) on top of the crosslinked poly(FA90-co-BFA10). Finally, a solution-processed red phosphorescent OLED device with the structure of indium tin oxide/poly(FA90-co-BFA10)/poly-TPD/emissive layer/TPBi/LiF/Al was fabricated and characterized. The device showed a low turn-on voltage (Von) of 3.5 V, a reasonably high current efficiency (CE) of 16.6 cd/A, and an external quantum efficiency (EQE) of 12.5 %, which are better than those of the corresponding reference device using PEDOT:PSS as the HIL. Moreover, the device fabricated using the poly(FA90-co-BFA10) HIL demonstrated a longer lifetime than that fabricated using PEDOT:PSS.