Unraveling the Stable Cathode Electrolyte Interface in all Solid-State Thin-Film Battery Operating at 5 V

Document Type
Publications · Journal Article
Registered DB
SCIEScopus
Journal Ranking
JCR Q1Scopus Q1
Journal
ADVANCED ENERGY MATERIALS12(31) · #2201119 · 2022
Citation
Web of Science 57Scopus 58
FWCI (Scopus)
2.06
JCR IF
JCR 2021 29.698
ISSN
1614-6832

Authors

  1. Shimizu, RyosukeFirst authorUniv Calif San Diego, Dept NanoEngn, La Jolla, CA 92093 USA
  2. Cheng, DiyiUniv Calif San Diego, Mat Sci & Engn Program, La Jolla, CA 92093 USA
  3. Weaver, Jamie L.NIST, Mat Measurement Lab, 100 Bur Dr, Gaithersburg, MD 20899 USA
  4. Zhang, MinghaoCorresponding authorUniv Calif San Diego, Dept NanoEngn, La Jolla, CA 92093 USA
  5. Lu, BingyuUniv Calif San Diego, Dept NanoEngn, La Jolla, CA 92093 USA
  6. Wynn, Thomas A.Univ Calif San Diego, Dept NanoEngn, La Jolla, CA 92093 USA
  7. Burger, RandallUniv Calif San Diego, Dept NanoEngn, La Jolla, CA 92093 USA
  8. Kim, Min-cheolPusan Natl Univ, Sch Mech Engn, Busan 46241, South Korea
  9. Zhu, GuominUniv Calif San Diego, Dept NanoEngn, La Jolla, CA 92093 USA
  10. Meng, Ying ShirleyCorresponding authorUniv Calif San Diego, Dept NanoEngn, La Jolla, CA 92093 USA

Abstract

Spinel-type LiNi0.5Mn1.5O4 (LNMO) is one of the most promising 5 V-class cathode materials for Li-ion batteries that can achieve high energy density and low production costs. However, in liquid electrolyte cells, the high voltage causes continuous cell degradation through the oxidative decomposition of carbonate-based liquid electrolytes. In contrast, some solid-state electrolytes have a wide electrochemical stability range and can withstand the required oxidative potential. In this work, a thin-film battery consisting of an LNMO cathode with a solid lithium phosphorus oxynitride (LiPON) electrolyte is tested and their interface before and after cycling is characterized. With Li metal as the anode, this system can deliver stable performance for 600 cycles with an average Coulombic efficiency >99%. Neutron depth profiling indicates a slight overlithiated layer at the interface prior to cycling, a result that is consistent with the excess charge capacity measured during the first cycle. Cryogenic electron microscopy further reveals intimate contact between LNMO and LiPON without noticeable structure and chemical composition evolution after extended cycling, demonstrating the superior stability of LiPON against a high voltage cathode. Consequently, design guidelines are proposed for interface engineering that can accelerate the commercialization of a high voltage cell with solid or liquid electrolytes.

Keywords

cathode electrolyte interphasecryogenic electron microscopyhigh-voltage spinel cathodesLi metal batteriesLiPONLITHIUM-ION BATTERIESTRANSITION-METAL DISSOLUTIONHIGH-VOLTAGE SPINELLINI0.5MN1.5O4 CATHODESOXYGEN VACANCIESSTABILITYPERFORMANCEADDITIVESCAPACITYLNMO/GRAPHITE