Influence of preliminary metal-ion etching on the topography and mechanical behavior of TiAlN coatings on cemented carbides
- Document Type
- Publications · Journal Article
- Registered DB
- SCIEScopus
- Journal Ranking
- JCR Q1Scopus Q1
- Journal
- SURFACE & COATINGS TECHNOLOGY432 · 2022
- Citation
- Web of Science 35Scopus 38
- FWCI (Scopus)
- 2.24
- JCR IF
- JCR 2021 4.865
- ISSN
- 0257-8972
Authors
- Peng, BinFirst authorGuangdong Univ Technol, Sch Electromech Engn, Guangzhou 510006, Peoples R China
- Xu, Yu X.Corresponding authorGuangdong Univ Technol, Sch Electromech Engn, Guangzhou 510006, Peoples R China
- Du, Jian W.Cent South Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
- Chen, LiCent South Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
- Kim, Kwang HoPusan Natl Univ, Global Frontier R&D Ctr Hybrid Interface Mat, Busan 609735, South Korea
- Wang, Qi MinCorresponding authorGuangdong Univ Technol, Sch Electromech Engn, Guangzhou 510006, Peoples R China
Abstract
© 2022 Elsevier B.V.Metal-ion etching is widely used in substrate surface modification before coating by physical vapor deposition. In this work, TiAlN coatings were synthesized onto cemented carbides with Ti-, Cr-, and Zr-ion pre-etching by cathodic arc evaporation and investigated concerning surface topography and mechanical failure. The pre-etching of energetic metal ions introduces droplet defects and increases surface roughness through uneven bombardment. The high interface roughness and deposition of nanoscale metal interlayers contributed to the upgraded adhesion between the coating and the substrate. As a result, the adhesion strength of TiAlN coatings advances to more than 95 N by applying Cr- and Zr-ion pre-etching. The rough substrate surface also gives rise to a rough coating surface associated with the pre-etching time. Under normal loading, the microscopic pit-like surface morphology, stemming from ion etching, interrupts the transverse propagation of the circumferential cracks but does not affect the longitudinal crack propagation inside the coating. In addition, the higher roughness of coatings with ion pre-etching causes a shorter run-in stage during ball-on-disc tests due to the higher contact stress between the friction pair.
Keywords
Crack propagationDry frictionIon etchingScratch adhesionSurface topographyHIGH-SPEED STEELSCRATCH ADHESIONHARD COATINGSCUTTING PERFORMANCESURFACE-TOPOGRAPHYRESIDUAL-STRESSESDROPLET FORMATIONNITRIDE COATINGSGROWTH DEFECTSTIN COATINGS