Fatigue Variability of Alloy 625 Thin-Tube Brazed Specimens
- Document Type
- Publications · Journal Article
- Registered DB
- SCIEScopus
- Journal Ranking
- JCR Q2Scopus Q2
- Journal
- METALS11(8) · #1162 · 2021
- Citation
- Web of Science 3Scopus 3
- FWCI (Scopus)
- 0.15
- JCR IF
- JCR 2020 2.351
- ISSN
- 2075-4701
Authors
- Lee, Seul BiFirst authorPusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
- Kim, HanjongPusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
- Park, SeonghunCorresponding authorPusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
- Choi, Yoon SukCorresponding authorPusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
Abstract
As an advanced heat exchanger for aero-turbine applications, a tubular-type heat exchanger was developed. To ensure the optimum performance of the heat exchanger, it is necessary to assess the structural integrity of the tubes, considering the assembly processes such as brazing. In this study, fatigue tests at room temperature and 1000 K were performed for 0.135 mm-thick alloy 625 tubes (outer diameter of 1.5 mm), which were brazed to the grip of the fatigue specimen. The variability in fatigue life was investigated by analyzing the locations of the fatigue failure, fracture surfaces, and microstructures of the brazed joint and tube. At room temperature, the specimens failed near the brazed joint for high sigma(max) values, while both brazed joint failure and tube side failure were observed for low sigma(max) values. The largest variability in fatigue life under the same test conditions was found when one specimen failed in the brazed joint, while the other specimen failed in the middle of the tube. The specimen with brazed joint failure showed multiple crack initiations circumferentially near the surface of the filler metal layer and growth of cracks in the tube, resulting in a short fatigue life. At 1000 K, all the specimens exhibited failure in the middle of the tube. In this case, the short-life specimen showed crack initiation and growth along the grains with large through thickness in addition to multiple crack initiations at the carbides inside the tube. The results suggest that the variability in the fatigue life of the alloy 625 thin-tube brazed specimen is affected by the presence of the brazed joint, as well as the spatial distribution of the grain size and carbides.
Keywords
fatigue variabilityalloy 625thin tubefractographymicrostructureLOW-CYCLE FATIGUEHIGH-EFFICIENCYTEMPERATURESUPERALLOYJOINTSSOLIDIFICATIONPERFORMANCEBEHAVIOR