Skip to content

Cold Cracks in Fillet Weldments of 600 MPa Tensile Strength Low Carbon Steel and Microstructural Effects on Hydrogen Embrittlement Sensitivity and Hydrogen Diffusion

인장강도 600 MPa급 저탄소강 필렛 용접부의 저온균열과 미세조직에 따른 수소취성 민감성 및 수소확산 거동

Document Type
Publications · Journal Article
Registered DB
KCISCIEScopus
Journal Ranking
JCR Q4Scopus Q2KCI Q1
Journal
Korean Journal of Metals and Materials59(1) · pp.21 · 2021
Citation
Web of Science 9Scopus 9KCI 4
FWCI (Scopus)
0.67
JCR IF
JCR 2020 1.005
ISSN
1738-8228

Authors

  1. An Hyoung JinFirst authorDepartment of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea
  2. Lee, JunghoonKIURI Institute, Yonsei University, Seoul 03722, Republic of Korea
  3. Park HanjiDepartment of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea
  4. Yoo, JaeSeokDaewoo Shipbuilding & Marine Engineering Co., Ltd., Department of Welding Engineering R&D, Geoje-si 53302, Republic of Korea
  5. Chung, SungwookDaewoo Shipbuilding & Marine Engineering Co., Ltd., Department of Welding Engineering R&D, Geoje-si 53302, Republic of Korea
  6. Park, JongminDaewoo Shipbuilding & Marine Engineering Co., Ltd., Department of Welding Engineering R&D, Geoje-si 53302, Republic of Korea
  7. Kang, NamhyunCorresponding authorDepartment of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea

Abstract

Hydrogen flowing into a weld causes hydrogen embrittlement (HE), so to prevent cold cracks in the weld, HE must be suppressed. In this study, single-pass fillet weldments were fabricated using two different welding fillers with the same strength level as the American Welding Society standard. The specimen F-HNi, which had a high, reversible hydrogen content, exhibited cold cracking in the fillet weld. The HE sensitivity index (HE index) was calculated using the in-situ slow strain rate test (SSRT). The reversible hydrogen trap concentration (C-rev) and hydrogen diffusion coefficient (D-eff) were calculated using the permeation test. The formation of low-temperature transformation phases such as bainite and martensite increased the C-rev and decreased the D-eff, thereby increasing the HE index. In addition, it was determined that reversible hydrogen was most effectively trapped in the low-temperature transformation phase, as confirmed by silver decoration. We concluded that the cold cracks in the F-HNi specimen were associated with the large C-rev, small D-eff, and large HE index. HE sensitivity can be controlled by optimizing the microstructure, even when welding fillers with the same level of strength are used. To reduce HE sensitivity, it is important to reduce the number of reversible hydrogen trap sites, by reducing the fraction of the low-temperature transformation phase where the reversible hydrogen trapping most occurs.

Keywords

weld metalhydrogen embrittlementhydrogen diffusionhydrogen trappingMETAL ARC WELDSACICULAR FERRITEDELAYED FRACTURESUSCEPTIBILITYSTRESSMNNIDISLOCATIONTEMPERATUREPERMEATION

Identifiers

Scopus EID
2-s2.0-85099884401
WoS UID
000610387400004
KCI