Effects of Mg and Sb Substitution on the Magnetic Properties of Magnetic Field Annealed MnBi Alloys

Document Type
Publications · Journal Article
Registered DB
SCIEScopus
Journal Ranking
JCR Q2Scopus Q2
Journal
NANOMATERIALS10(11) · 2020
Citation
Web of Science 10Scopus 11
FWCI (Scopus)
0
JCR IF
JCR 2019 4.324
ISSN
2079-4991

Authors

  1. Qian, Hui-DongFirst authorSchool of Materials Science and Engineering, Pusan National University, Busan, 46241, Korea
  2. Yang YangSchool of Materials Science and Engineering, Pusan National University, Busan, 46241, Korea
  3. Lim, Jung TaePowder & Ceramics Division, Korea Institute of Materials Science, Changwon, 51508, Korea;
  4. Kim, Jong-WooPowder & Ceramics Division, Korea Institute of Materials Science, Changwon, 51508, Korea;
  5. Choi, Chul-JinCorresponding authorPowder & Ceramics Division, Korea Institute of Materials Science, Changwon, 51508, Korea;
  6. Park, JihoonCorresponding authorPowder & Ceramics Division, Korea Institute of Materials Science, Changwon, 51508, Korea;

Abstract

Rare-earth-free permanent magnets have attracted considerable attention due to their favorable properties and applicability for cost-effective, high-efficiency, and sustainable energy devices. However, the magnetic field annealing process, which enhances the performance of permanent magnets, needs to be optimized for different magnetic fields and phases. Therefore, we investigated the effect of composition on the crystallization of amorphous MnBi to the ferromagnetic low-temperature phase (LTP). The optimal compositions and conditions were applied to magnetic field annealing under 2.5 T for elemental Mg- and Sb/Mg pair-substituted MnBi. The optimum MnBi composition for the highest purity LTP was determined to be Mn56Bi44, and its maximum energy product, (BH)(max), was 5.62 MGOe. The Mg-substituted MnBi exhibited enhanced squareness (M-r/M-s), coercivity (H-c), and (BH)(max) values up to 0.8, 9659 Oe, and 5.64 MGOe, respectively, whereas the same values for the Sb/Mg pair-substituted MnBi were 0.76, 7038 Oe, and 5.60 MGOe, respectively. The substitution effects were also investigated using first-principles calculations. The density of states and total magnetic moments of Mn16Bi15Mg and Mn16Bi15Sb were similar to those of pure Mn16Bi16. Conversely, the Sb-substituted MnBi resulted in a dramatic enhancement in the anisotropy constant (K) from a small negative value (-0.85 MJ/m(3)) to a large positive value (6.042 MJ/m(3)).

Keywords

MnBiMg substitutionSb substitutionmagnetic propertiesmagnetic field annealingELECTRONIC-STRUCTURECRYSTAL-STRUCTUREHIGH COERCIVITYMICROSTRUCTURE