Characteristics according to the Amount of HAp Added in Resin for Tooth Repair

Document Type
Publications · Review Article
Registered DB
KCISCIEScopus
Journal Ranking
Scopus Q3
Journal
JOURNAL OF THE KOREAN CERAMIC SOCIETY56(6) · pp.521 · 2019
Citation
Web of Science 1Scopus 1KCI 1
FWCI (Scopus)
0.02
ISSN
1229-7801

Authors

  1. Hwang, SunguFirst authorDepartment of Nanomechatronics Engineering, Pusan National University, Busan 46241, Korea
  2. Jinhyuck LimDepartment of Nanomechatronics Engineering, Pusan National University, Busan 46241, Korea
  3. Ryu, Su ChakCorresponding authorDepartment of Nanomechatronics Engineering, Pusan National University, Busan 46241, Korea

Abstract

A study was conducted to investigate the possibility of a composite material containing a composite resin as a matrix and hydroxyapatite (HAp) powder as a substitute material for tooth repair. As the content of HAp increased, hardness value (111.9 HV at 9%) increased and flexural strength (73.3 MPa at 9%) decreased. Observation of the microstructure after immersion in a simulated body fluid (SBF) solution confirmed a dense structure due to mutual coagulation and curing. It was thought that fine HAp recrystals were formed with the lapse of time, and they were entangled to form a condensation structure and had a dense structure. In addition, since the activity was shown by the ion migration on the surface of a tooth, it was highly likely that a biocompatible bond occurred during tooth contact. Therefore, it could be used as a substitute material for tooth repair.

Keywords

HydroxyapatiteCompositeRepairResinTooth