Effect of different sizes of bioactive glass-coated mesoporous silica nanoparticles on dentinal tubule occlusion and mineralization

Document Type
Publications · Journal Article
Registered DB
SCIEScopus
Journal Ranking
JCR Q1Scopus Q1
Journal
CLINICAL ORAL INVESTIGATIONS23(5) · pp.2129 · 2019
Citation
Web of Science 33Scopus 39
FWCI (Scopus)
1.9
JCR IF
JCR 2018 2.453
ISSN
1432-6981

Authors

  1. Jung, Jae HyunFirst authorDepartment of Orthodontics, Dental Research Institute, Pusan National University Dental Hospital, Geumoro 20, Mulgeum, Yangsan, 50612, South Korea
  2. Park, SoobyungDepartment of Orthodontics, Dental Research Institute, Pusan National University Dental Hospital, Geumoro 20, Mulgeum, Yangsan, 50612, South Korea
  3. Yoo, Kyung-HyeonSchool of Materials Science and Engineering, Pusan National University, Busandaehak-ro 63beon-gil, Geumjeong-gu, Busan, 46241, South Korea
  4. Yoon, Seog YoungSchool of Materials Science and Engineering, Pusan National University, Busandaehak-ro 63beon-gil, Geumjeong-gu, Busan, 46241, South Korea
  5. Bae, Moon KyoungDepartment of Oral Physiology, School of Dentistry, Pusan National University, Busandaehak-ro 49, Mulgeum, Yangsan, 50612, South Korea
  6. Lee, Dong JoonDepartment of Orthodontics, School of Dentistry, University of North Carolina, Chapel Hill, NC, 27599, USA
  7. Ko, Ching-ChangDepartment of Orthodontics, School of Dentistry, University of North Carolina, Chapel Hill, NC, 27599, USA
  8. Kwon, YounghoonDepartment of Dental Materials, Pusan National University, Busandaehak-ro 49, Mulgeum, Yangsan, 50612, South Korea
  9. Kim, YongilCorresponding authorDepartment of Orthodontics, Dental Research Institute, Pusan National University Dental Hospital, Geumoro 20, Mulgeum, Yangsan, 50612, South Korea

Abstract

ObjectivesTo synthesize two different sizes of bioactive glass-coated mesoporous silica nanoparticles (BGN@MSNs) and to investigate their effects on dentinal tubule occlusion and remineralization.Materials and methodsTwo different sizes of mesoporous silica nanoparticles (MSNs) were synthesized using the Stober method (368A, 1840A) and coated with bioactive glass nanoparticles (BGNs) using a modified quick alkali-mediated sol-gel method (368B, 1840B). Sensitive tooth disc models were prepared and divided into six groups and the following treatments were applied: group 1no treatment, group 2bioglass, group 3368A, group 4368B, group 51840A, and group 61840B. Then, five discs were selected from each group and soaked in 6wt% citric acid to test acid resistance. Dentinal tubule occlusion and occlusion ratio were observed using field-emission scanning electron microscopy. In vitro mineralization tests using simulated body fluid solution were performed to evaluate the remineralization effect of the treatment.ResultsAll samples effectively occluded the dentinal tubule and formed a membrane-like layer. After acid treatment, 1840B (group 6) exhibited the highest rate of dentinal tubule occlusion. Remineralization was observed in 368B and 1840B, and 1840B exhibited the fastest remineralization.ConclusionsDentinal tubule remineralization induced by the BGN@MSN biocomposite can be used to stabilize long-term prognosis in dentin hypersensitivity. The 1840B induced the most efficient remineralization, and its smaller size and larger surface area were effective for remineralization.Clinical relevanceThe BGN@MSN biocomposite with its smaller size and larger surface area was more effective for remineralization and dentinal tubule sealing.

Keywords

Bioactive glassMesoporous silicaSizeSurface areaNanoparticleRemineralizationDentin hypersensitivityHYPERSENSITIVITYPERMEABILITYACIDSEM