Investigation of surface defects of electroless Ni plating by solder resist dissolution on the ENIG process
- Document Type
- Publications · Journal Article
- Registered DB
- SCIEScopus
- Journal Ranking
- JCR Q2Scopus Q1
- Journal
- MICROELECTRONIC ENGINEERING200 · pp.39 · 2018
- Citation
- Web of Science 8Scopus 11
- FWCI (Scopus)
- 0.18
- JCR IF
- JCR 2017 2.02
- ISSN
- 0167-9317
Authors
- Leehyun, JuFirst authorDepartment of Mechanical Engineering, Worcester Polytechnic Institute, Worcester, United States
- Lee, SeungjunManufacture Team, LCR Division, Samsung Electro-Mechanics, Suwon, South Korea
- Kim, KaheeDepartment of Advanced Circuit Interconnection, Pusan National University, Busan, South Korea
- Heo, CheolhoFCB team, ACI Division, Samsung Electro-Mechanics, Busan, South Korea
- Lee, Jae-HoCorresponding authorDepartment of Materials Science and Engineering, Hongik University, Seoul, South Korea
- Kim, YangdoSchool of Materials Science and Engineering, Pusan National University, Busan, South Korea
Abstract
Defects, such as a black pads and pinholes, are generated on the Ni/Au interface after the electroless nickel immersion gold (ENIG) process. The contamination of plating solutions, including dissolution of the solder resist (SR), side reaction products, and impurities (Cu, Ni, drag-in), can be a cause of the black pad phenomenon. In this study, electroless Ni plating was investigated to determine the correlation between SR dissolution and black pad generation. Three different SR components, monomer, hardener, and photoinitiator were used to examine the effects of the properties of the coating layer. The surface morphology, plating rate, and phosphorus (P) content of the electroless Ni layer with SR additives were analyzed. The black pad mechanism by SR dissolution was examined by electrochemical analysis including the open circuit voltage (OCV) and cyclic voltammetry (CV) in a three-electrode cell. When a few ppm of SR was added, the OCV increased compared to the pure solution. CV revealed a change in hysteresis loop in the oxidation region upon the addition of SR. The contamination in the solution promotes the oxidation reaction rather than the reduction reaction. Therefore, the content of P in the contaminated solution was higher than that of the pure solution, and defects, such as black pad and pinholes, were observed.
Keywords
Electroless nickel immersion goldSurface defectsSolder resistBlack padCyclic voltammetryNICKEL-IMMERSION GOLDBLACK PAD PHENOMENONPACKAGESFINISHESFAILUREJOINTS