Skip to content

Effect of Austenite-to-Ferrite Phase Transformation at Grain Boundaries on PWHT Cracking Susceptibility in CGHAZ of T23 Steel

Document Type
Publications · Journal Article
Registered DB
SCIEScopus
Journal Ranking
JCR Q2Scopus Q3
Journal
METALS8(6) · 2018
Citation
Web of Science 2Scopus 4
FWCI (Scopus)
0.09
JCR IF
JCR 2017 1.704
ISSN
2075-4701

Authors

  1. Lee Seong HyeongFirst authorDepartment of Hybrid Materials & Machining Technology, Graduate School of Convergence Science, Pusan National University, Busan, South Korea
  2. Na, Hye SungDepartment of Material Science and Engineering, Pusan National University, Busan, South Korea
  3. Lee, Kyong-WoonCorporate R&D Institute, Doosan Heavy Industries, Changwon, South Korea
  4. Lee, Jeong-YongDepartment of Material Science and Engineering, Pusan National University, Busan, South Korea
  5. Kang, ChungyunCorresponding authorDepartment of Material Science and Engineering, Pusan National University, Busan, South Korea

Abstract

The post-weld heat treatment (PWHT) cracking susceptibility of a coarse grain heat-affected zone (CGHAZ) in SA213-T23 (2.25Cr-1.6W steel) that was used for boiler tubes employed in thermal power plants was investigated using a Gleeble thermal cycle simulator. The PWHT cracking susceptibility test was performed at 650 degrees C, 700 degrees C, and 750 degrees C, and it can be judged that the lower the reduction of the area, the more susceptible it is to PWHT cracking. The results of the test also showed higher cracking susceptibility at 650 degrees C and 700 degrees C, which mostly involved intergranular fracture, while at 750 degrees C, transgranular fracture was exhibited. Therefore, the PWHT cracking susceptibility is considered to be closely related to grain boundary. The microstructure of the simulated CGHAZ and PWHT at 650 degrees C, 700 degrees C, and 750 degrees C was observed after etching with nital and alkaline sodium picrate etchants. Alkaline sodium picrate-etched microstructures showed a white band at the grain boundary at 650 degrees C, 700 degrees C, and 750 degrees C, which did not appear in nital etching. An analysis of the white band using an electron probe micro-analyzer (EPMA), TEM, and nanoindentation revealed that it was intergranular ferrite depleted with C, W, and Cr as compared with that in the matrix. Based on these results, we investigated the mechanism of intergranular ferrite formation during PWHT and its effect on PWHT cracking susceptibility at 650 degrees C, 700 degrees C, and 750 degrees C.

Keywords

SA213-T23Cr-Mo steelCGHAZPWHT crackingintergranular ferritetint etchingINTERGRANULAR CRACKINGELEVATED-TEMPERATURESWELD METALSMICROSTRUCTUREBEHAVIORZONETI

Identifiers

Scopus EID
2-s2.0-85048124522
WoS UID
000436115600044