Skip to content

Study on the Formation of Reaction Phase to Si Addition in Boron Steel Hot-Dipped in Al-7Ni Alloy

Document Type
Publications · Journal Article
Registered DB
SCIEScopus
Journal Ranking
JCR Q2
Journal
COATINGS7(11) · 2017
Citation
Web of Science 12Scopus 12
FWCI (Scopus)
0.44
JCR IF
JCR 2016 2.175
ISSN
2079-6412

Authors

  1. Yun, Jung-GilFirst authorDepartment of Hybrid Materials and Machining Technology, Graduate School of Convergence Science, Pusan National University, Busan, South Korea
  2. Lee, Jae hyeongDepartment of Material Science and Engineering, Pusan National University, Busan, South Korea
  3. Kwak, Sung-YunDepartment of Material Science and Engineering, Pusan National University, Busan, South Korea
  4. Kang, ChungyunCorresponding authorDepartment of Material Science and Engineering, Pusan National University, Busan, South Korea

Abstract

In order to reduce the intermetallic compounds formed during the application of an Al-7Ni wt % hot-dip multifunctional coating on boron steel, developed for Tailor Welded Blanks (TWB) and hot stamping, 2-6 wt % Si was added to the coating to change the reaction layer. The coating was run at 690 degrees C for 120 s. Al9FeNi phases were formed on the steel interface, Fe2Al5 was formed on the steel, FeAl3 was generated between the existing layers, and flake-type Al2Fe3Si3 was formed in the Fe2Al5 phase, depending on the Si content. In addition, as Si was added to the coating, the thickness of the Fe2Al5 phase decreased and the thickness of the Al9FeNi phase and Al2Fe3Si3 increased. The decrease in the thickness of the Fe2Al5 phase was mainly due to the effect of the Si solid solution and the Al2Fe3Si3 formation in the Fe2Al5 phase. The reason for the growth of Al9FeNi is that the higher the Si content in the coating, the more the erosion of the interface of the steel material due to the coating solution. Therefore, the outflow of Fe into the coating liquid increased.

Keywords

hot-dipped coatingaluminized steelFe-Al-Ni phaseFe-Al-Si phasereduced intermetallicsadvanced high-strength steelTailor Welded Blanks (TWB)hot-stampingGROWTH-KINETICSMICROSTRUCTURESILICONJOINTSSHEET