Fabrication and energy harvesting characteristics of unimorph piezoelectric cantilever generators with interdigitated electrode lead zirconate titanate laminates
- Document Type
- Publications · Journal Article
- Registered DB
- SCIEScopus
- Journal Ranking
- JCR Q3Scopus Q1
- Journal
- JAPANESE JOURNAL OF APPLIED PHYSICS56(12) · 2017
- Citation
- Web of Science 5Scopus 7
- FWCI (Scopus)
- 0.39
- JCR IF
- JCR 2016 1.384
- ISSN
- 0021-4922
Authors
- Min-seon LeeFirst authorDepartment of Materials Science and Engineering, Pusan National University, Busan, South Korea
- Yun, Ji-SunElectronic Convergence Materials Division, Korea Institute of Ceramic Engineering and Technology, Jinju, Gyeongnam, South Korea
- Park, Woon-IkElectronic Convergence Materials Division, Korea Institute of Ceramic Engineering and Technology, Jinju, Gyeongnam, South Korea
- Hong, Youn-WooElectronic Convergence Materials Division, Korea Institute of Ceramic Engineering and Technology, Jinju, Gyeongnam, South Korea
- Jeongho ChoElectronic Convergence Materials Division, Korea Institute of Ceramic Engineering and Technology, Jinju, Gyeongnam, South Korea
- Paik, Jong-HooElectronic Convergence Materials Division, Korea Institute of Ceramic Engineering and Technology, Jinju, Gyeongnam, South Korea
- Park, YonghoDepartment of Materials Science and Engineering, Pusan National University, Busan, South Korea
- Son, Chun-MyungKEPCO KDN Co., Ltd., Jeonnam, Naju, South Korea
- Jeong, Young HunCorresponding authorElectronic Convergence Materials Division, Korea Institute of Ceramic Engineering and Technology, Jinju, Gyeongnam, South Korea
Abstract
Interdigitated electrode (IDE) unimorph piezoelectric cantilever generators (UPCGs) were fabricated and their energy harvesting characteristics were investigated. A hard lead zirconate titanate (PZT) material with a high mechanical quality factor (Q(m)) of 1280 was used for the active piezoelectric film of the IDE UPCGs. Two different laminated IDE UPCGs were prepared; one has Ag/Pd interdigitated electrode (IDE) formed only on the top and bottom PZT sheets (D-IDE), while the other has Ag/Pd IDE on all of the PZT sheets (M-IDE). Cofiring was conducted at 1050 degrees C for 2 h for PZT laminates with IDEs. The fabricated IDE UPCGs exhibited power densities of 50.4 mu W/cm(3) for the D-IDE and 820 mu W/cm(3) for the M-IDE. The UPCG with the M-IDE exhibited a higher performance than that with the D-IDE. Specifically, a significantly enhanced normalized power factor of 670 mu W/(g(2).cm(3)) was found at 118Hz across 100 k Omega. (c) 2017 The Japan Society of Applied Physics
Keywords
Identifiers
- Scopus EID
- 2-s2.0-85039161420
- WoS UID
- 000415862500001



Login
Back to Publication list