Effect of Chloride Precursors on the Stability of Solution-Processed Indium Zinc Oxide Thin-Film Transistors
- Document Type
- Publications · Journal Article
- Registered DB
- SCIEScopus
- Journal Ranking
- JCR Q3Scopus Q1
- Journal
- JAPANESE JOURNAL OF APPLIED PHYSICS52(10) · 2013
- Citation
- Web of Science 9
- JCR IF
- JCR 2012 1.067
- ISSN
- 0021-4922
Authors
- Lee, Dong HeeFirst authorDepartment of Electronics, Pusan National University, South Korea
- Park, Sung-MinDepartment of Electronics, Pusan National University, South Korea
- Yang, JungilDepartment of Electronics, Pusan National University, South Korea
- Cho, DongkyuDepartment of Electronics, Pusan National University, South Korea
- Woo, SanghyunDepartment of Electronics, Pusan National University, South Korea
- Lim, YooseongDepartment of Electronics, Pusan National University, South Korea
- Kim, Dae KukDepartment of Electronics, Pusan National University, South Korea
- Yi, MoonsukCorresponding authorDepartment of Electronics, Pusan National University, South Korea
Abstract
In this experiment, solution-processed indium zinc oxide (IZO) films were prepared by spin-coating the films as an active layer in thin-film transistors (TFTs). These films were coated with nitrate and a mixture of acetate-and chloride-based precursors to allow the IZO films to contain indium and zinc components. The solution-processed IZO-based TFT fabricated using a zinc acetate precursor for the IZO films exhibited a mobility of 2.83 cm(2) V-1 s(-1), an on/off current ratio of similar to 1 x 10(5), and a subthreshold swing value of 2.48 V/dec. The IZO-TFT with the zinc chloride precursor exhibited a mobility of 4.37 cm(2) V-1 s(-1), an on/off current ratio of similar to 1 x 10(3), and a subthreshold swing value of 6.44 V/dec. In comparison, the IZO-TFT with a mixture of zinc acetate and chloride precursors exhibited a mobility of 1.45 cm(2) V-1 s(-1), an on/off current ratio of similar to 1 x 10(5), and a subthreshold swing value of 1.83 V/dec. The first two devices suffered from a large threshold voltage (Vth) shift, >7 and >6 V, respectively, after a gate voltage of 20 V was applied for 2 h. In contrast, the device fabricated using the mixed precursors showed a higher stability, shifting about 1.7V under the same stress conditions. (C) 2013 The Japan Society of Applied Physics
Keywords
ROOM-TEMPERATUREELECTRICAL-PROPERTIESHIGH-PERFORMANCECHANNEL LAYERZNOSEMICONDUCTOR