Synthesis and characterization of low-bandgap copolymers based on dihexyl-2H-benzimidazole and terthiophene
- Document Type
- Publications · Journal Article
- Registered DB
- SCIEScopus
- Journal Ranking
- JCR Q1
- Journal
- SYNTHETIC METALS160(23-24) · pp.2618 · 2010
- Citation
- Web of Science 9
- JCR IF
- JCR 2009 1.901
- ISSN
- 0379-6779
Authors
- Song, SuheeFirst authorDepartment of Chemistry, Chemistry Institute for Functional Materials, Pusan National University, South Korea
- Park, Sung HeumDepartment of Materials Science and Engineering, Gwangju Institute of Science and Technology, South Korea
- Jin, YoungeupDepartment of Industrial Chemistry, Pukyong National University, South Korea
- Goo, YoungranDepartment of Chemistry, Chemistry Institute for Functional Materials, Pusan National University, South Korea
- Kim, IlWCU Center for Synthetic Polymer Bioconjugate Hybrid Materials, Department of Polymer Science and Engineering, Pusan National University, South Korea
- Lee, HeesooSchool of Materials Science and Engineering, Pusan National University, South Korea
- Lee, KwangheeDepartment of Materials Science and Engineering, Gwangju Institute of Science and Technology, South Korea
- Suh, HongsukCorresponding authorDepartment of Chemistry, Chemistry Institute for Functional Materials, Pusan National University, South Korea
Abstract
A series of new semiconducting polymers with 3-(hexyloxy)thiophene, 2,2-dihexyl-2H-benzimidazole (HBI) and thiophene units was synthesized using Stille polymerization. These random copolymers show good solubility at room temperature in organic solvents owing to the long alkyl chain in new acceptor, 2,2-dihexyl-2H-benzimidazole. In HBI, the sulfur at 2-position of 2,1,3-benzothiadiazole (BT) unit was replaced with the carbon to make a highly soluble electron deficient moiety while keeping the 1,2-quinoid form of BT unit. The spectra of the solid films show absorption bands with maximum peaks at about 408-526 nm and the absorption onsets at 550-692 nm, corresponding to band gaps of 1.79-2.25 eV. The onset wavelengths of the absorption spectra in thin films exhibit a gradual red-shift with decreased amount of dihexyl-2H-benzimidazol unit, that is, from 550 nm with PHOTDTHBI-9 to 692 nm with PHOTDTHBI-1. Under white light illumination (AM 1.5G. 100 mW/cm(2)), the device with PHOTDTHBI-3:PCBM blend demonstrated a V-OC value of 0.36 V. a J(SC) value of 1.20 mA/cm(2), and a FF of 0.37, leading to the efficiency of 0.16%. Crown Copyright (C) 2010 Published by Elsevier B.V. All rights reserved.
Keywords
PolymerPhotovoltaic cellsThiophene2H-benzimidazoleSOLAR-CELLSCONJUGATED POLYMERSCONDUCTING POLYMERPOLY(3-ALKYLTHIOPHENES)POLYTHIOPHENESDERIVATIVESDESIGNSTATE
Identifiers
- WoS UID
- 000286910000038



Login
Back to Publication list