Characteristics of amorphous Yb-doped ITO films deposited on polyimide substrate by DC magnetron sputtering

Document Type
Publications · Conference Paper
Registered DB
SCIEScopus
Journal Ranking
JCR Q1
Journal
SURFACE & COATINGS TECHNOLOGY205 · pp.S318 · 2010
Citation
Web of Science 4
JCR IF
JCR 2009 1.793
ISSN
0257-8972

Authors

  1. Jung, TaedongFirst authorNational Core Research Center for Hybrid Materials Solution, Pusan National University, South Korea
  2. Kim, SeilDepartment of Materials Science and Engineering, Pusan National University, South Korea
  3. Song, PungkeunCorresponding authorDepartment of Materials Science and Engineering, Pusan National University, South Korea

Abstract

The ITO and Yb-doped ITO (ITO:Yb) films were deposited on polyimide (PI) substrates by DC magnetron sputtering using ITO targets (doped-Yb: 0, 0.57, 3.2 and 7.75 at.%) containing different Yb ratios. Film deposition and post-annealing were carried out at room temperature and different temperatures (170 degrees C and 200 degrees C), respectively, in a pure Ar gas atmosphere at 1.0 Pa for 1 h. The ITO:Yb films had a higher crystallization temperature than that of the ITO films, which was attributed to Yb3+ atoms degrading the crystallinity of the ITO film. The ITO:Yb films also had good mechanical properties and a very flat surface morphology above the crystallization temperature of the ITO films (approximately 170 degrees C). The lowest resistivity of the polycrystalline ITO films obtained was 2.983 x 10(-4) Omega cm at 200 degrees C. On the other hand, the amorphous ITO:Yb films deposited from the 3.2 at.% Yb-doped ITO target at 170 degrees C had the lowest resistivity of 4.672 x 10(-4) Omega cm. The transmittance of all the ITO:Yb films was >80% in the visible region. (C) 2010 Elsevier B.V. All rights reserved.

Keywords

ITODC magnetron sputteringAmorphous TCOYb-dopedFlexible substrateHigh thermal durabilityTIN-OXIDE-FILMSINDIUM OXIDETHIN-FILMSTEMPERATURE